1、點(diǎn)膠機(jī)上膠閥滴漏這一場(chǎng)景在以后經(jīng)常發(fā)生在膠閥關(guān)閉時(shí)。95%的這些圖像是由于使用的針頭太小造成的。如果針頭太小,就會(huì)影響液體的運(yùn)動(dòng),形成反壓力。這一結(jié)果將導(dǎo)致橡膠閥關(guān)閉后不久出現(xiàn)滴漏現(xiàn)象。如果針筒過(guò)小,也會(huì)影響橡膠閥開(kāi)始使用時(shí)排氣氣泡的作用。錐形斜針的背壓小,流體運(yùn)動(dòng)平穩(wěn)。膠水閥關(guān)閉后,內(nèi)部液體空氣會(huì)滴漏。深圳點(diǎn)膠機(jī)生產(chǎn)廠家提倡,好提前清理內(nèi)部的液體空氣,或者使用不含氣泡的膠水,或者將膠水離心后使用。
1. The leakage of the glue valve on the dispenser often happens when the glue valve closes in the future. Ninety-five percent of these images were caused by the use of too small needles. If the needle is too small, it will affect the movement of the liquid, forming back pressure. This result will lead to leakage shortly after the rubber valve closes. If the syringe is too small, it will also affect the role of exhaust bubbles when rubber valves start to use. The conical oblique needle has the smallest back pressure and the smoothest fluid movement. When the glue valve closes, the internal liquid air will drip. Shenzhen dispensing machine manufacturers advocate that it is best to clean up the liquid air in advance, or use glue without bubbles, or centrifuge the glue after use.
2、分配器的尺寸不一致時(shí)膠料不一致,主要是由于儲(chǔ)油缸的流體壓力或氣壓不穩(wěn)定。進(jìn)氣壓力調(diào)節(jié)器應(yīng)該設(shè)置在比工廠小壓力低10到15psi的地方。壓力缸內(nèi)使用的壓力應(yīng)在調(diào)節(jié)閥壓力中心以上。壓力應(yīng)防止用于壓力表的低壓部分。橡膠閥門的工作壓力少為60psi,以保證膠水的穩(wěn)定性。后檢查上膠時(shí)間。如果小于15/1000秒,分配器的上膠時(shí)間會(huì)更穩(wěn)定。
2. When the size of distributor is different, the rubber material is different, mainly because of the unstable fluid pressure or air pressure of the oil storage cylinder. The intake pressure regulator should be set 10 to 15 psi below the minimum pressure of the plant. The pressure used in the pressure cylinder should be above the pressure center of the regulating valve. Pressure shall be prevented from low pressure parts used for pressure gauges. The working pressure of the rubber valve is at least 60psi to ensure the stability of the glue. Finally, check the gluing time. If less than 15/1000 seconds, the gluing time of the distributor will be more stable.
流量太慢了。如果流速過(guò)慢,管道應(yīng)由1/4“改為3/8”。管道越短越好。
The traffic is too slow. If the flow rate is too slow, the pipeline should be changed from 1/4 to 3/8. The shorter the pipe, the better.
4、點(diǎn)膠機(jī)液泡過(guò)大,液壓力過(guò)大,如果再加上閥門開(kāi)度過(guò)短,可能是空氣進(jìn)入液中,處理方法是降低液壓力,并采用錐形斜針。
4. The dispenser has too large bubbles and too large hydraulic pressure. If the opening of the valve is too short, it may be that air enters the liquid. The treatment method is to reduce the hydraulic pressure and adopt a conical oblique needle.
5、即時(shí)膠(快干膠)橡膠閥‘聯(lián)合’和管道塊看到主要是因?yàn)檫^(guò)多的水分或重復(fù)使用強(qiáng)力膠,應(yīng)保證新鮮即時(shí)膠水的使用,管道不徹底清潔的丙酮丙酮含有水分,應(yīng)該得出的結(jié)論是,使用空氣干燥和廠內(nèi)空氣壓力之間的橡膠閥系統(tǒng)和添加過(guò)濾器。(如果上述方法仍然失敗,則應(yīng)施用氮?dú)狻?
5. Instant glue (quick-drying glue) rubber valves and pipeline blocks are mainly due to excessive moisture or re-use of strong glue. Fresh instant glue should be guaranteed. Acetone and acetone which is not thoroughly cleaned in the pipeline contain moisture. It should be concluded that the rubber valve system between air drying and air pressure in the factory and the addition of filters should be used. If the above method still fails, nitrogen should be applied. )
6、UV膠(UV固化膠)確定使用黑線。不要直接添加UV膠老UV膠壓力缸,先把原來(lái)的UV膠水,然后把UV膠水到空壓力缸,增壓缸的UV膠通常通過(guò)一段時(shí)間后,泡沫和橡膠是不穩(wěn)定的。
6. UV adhesive (UV curing adhesive) determines the use of black line. Do not directly add UV glue to the old UV pressure cylinder, first put the original UV glue, then UV glue to the air pressure cylinder, and the UV glue of the pressurized cylinder usually passes through a period of time, and the foam and rubber are unstable.
7、針頭一般小于20針時(shí)可能會(huì)發(fā)生空氣問(wèn)題——滴水或垂直流動(dòng),一般盡量使用較大的金屬針或錐形斜針,防止使用創(chuàng)口或鐵氟隆針。
7. Air problems may occur when needles are usually less than 20 needles - dripping or vertical flow. Generally, larger metal needles or tapered oblique needles should be used as far as possible to prevent the use of wounds or Teflon needles.
8、環(huán)氧樹(shù)脂(環(huán)氧樹(shù)脂)清洗機(jī)廠家提倡,我們盡可能每班都用一般甲苯溶劑儲(chǔ)存壓力缸自動(dòng)清洗,越頻繁越好。
8. The manufacturer of Shenzhen Extension of Epoxy Resin (Epoxy Resin) Cleaning Machine advocates that we use general toluene solvent to store pressure cylinder for automatic cleaning in every shift, the more frequent the better.